לפניכם התקציר של המאמר:


Influence of food-simulating solutions and surface finish on susceptibility to staining of aesthetic restorative materials

R. Bagheri, M.F. Burrow and M. Tyas
School of Dental Science, University of Melbourne, Vic. 3010, Australia

Received 28 January 2004;  revised 12 October 2004;  accepted 20 October 2004.  Available online 9 December 2004.
Objectives
To determine the degree of surface staining of resin-based composites (RBCs) and glass-ionomer cements (GICs) after immersion in various stains and food-simulating solutions (FSS).
Methods
Six tooth-coloured restorative materials were used: a light-cured microfilled RBC (Durafil, Kulzer), a light-cured microglass RBC (Charisma, Kulzer), a polyacid-modified RBC (F2000, 3M/ESPE), a conventional GIC (Fuji IX, GC) and two resin-modified GICs (Fuji II LC, GC; Photac Fil, 3M/ESPE). Disk-shaped specimens were prepared and tested with either a matrix finish or polished using wet silicon carbide papers up to 2000 grit. All specimens were immersed in 37 °C distilled water for 1 week, followed by three different FSS (water, 10% ethanol, Crodamol GTCC) and five stains (red wine, coffee, tea, soy sauce and cola) for a further 2 weeks. Three specimens of each material for each stain were tested. Colour coefficients (CIE L* a* b*) were measured by a spectrophotometer after each treatment. The change in colour (ΔEn) was calculated using the formula: ΔEn=[(ΔLn+(Δan)2+(Δbn)2]1/2
Results
Distilled water caused no perceptible colour change as tested by ANOVA and Tukey’s tests. The effect of surface finish on staining was not statistically significant (P>0.05). There was no strong interaction between FSS and stains or between FSS and materials. There was a strong interaction between surface and material, and stain and material (P<0.001).
Conclusions
All materials were susceptible to staining by all stains especially coffee, red wine and tea; Fuji IX showed the least susceptibility and F2000 the greatest

תגובות רוצה להצטרף לדיון?

אין תגובות עדיין. היה הראשון להגיב!

מאמרים

בונדינג מהדור החדש

בונדינג מהדור החדש

מערכת האתר
מערכת האתר
אין תגובות|07/11/2004

בונדינג מהדור החדש -בקבוק אחד לכל-משמש כממברנה ולא אוטם את

כניסת צוות רפואי

הכניסה לאתר מותרת אך ורק לצוות הרפואי

לקבלת קוד אימות לנייד ולמייל, יש למלא את כתובת המייל ואת מספר הטלפון שלך

עדיין לא נרשמת? באפשרותך לבצע רישום כאן